Experimental and analytical analysis of punching shear in flat slabs supported on column topped with concrete head
PublikacjaAn experimental laboraatory test of the two series of slab-column elements topped with drop panels of varying sizes is described in this paper. The scope of the paper is to investigate the influence of the drop panel size and stiffness on the behaviour of the connection between the flat slab and the column topped by the concrete head. The impact of the head size and stiffness is analysed analytically and experimentally. The experimental...
-
Shear Cap Size Selection Method Based on Parametric Analysis of ACI-318 Code and Eurocode 2 Standard
PublikacjaThe scope of the paper is to propose a method for determining the size of shear caps in a slab–column-connections-reinforced concrete structure. Usually, shear heads are used to enhance slab–column connection, especially when the transverse reinforcement does not give the required punching shear load capacity. The dimensions of the shear head should provide the punching shear resistance of the connection inside and outside the...
-
Verification of punching shear outside the shear cap by the direct method
PublikacjaThe proposition of a method to verify the punching resistance for very large supports based on the EN 1992-1-1 standard is described in this paper. The present standard guidelines for the calculation of the punching resistance for large supports are also summarised. The proposed direct method is compared with other standard methods using an example taken from design practice. This method consists of a direct check of the shear...
-
Determination of changes in viscosity of hydrogel depending on shear rate (6.6 to 330 s-1).
Dane BadawczeThe rheological characteristics of hydrogel were made on the basis of a viscosity measurement using a Brookfield viscometer, using LV SC4 - 18 spindle and shear rates from 6.6 to 330 s-1.
-
Effect of lag screw on stability of first metatarsophalangeal joint arthrodesis with medial plate
PublikacjaBackground: First metatarsophalangeal joint (MTP-1) arthrodesis is a commonly performed procedure in the treatment of disorders of the great toe. Since the incidence of revision after MTP-1 joint arthrodesis is not insignificant, a medial approach with a medially positioned locking plate has been proposed as a new technique. The aim of the study was to investigate the effect of the application of a lag screw on the stability and...
-
Inflow of fly ash on selected geotechnical parameters of soft soils.
Dane BadawczeThe reaserch presents the experimental results made on samples of soft soils mixed with fly ash in different proportions (10%, 20%, 30%). The files contains the data directly from direct shear aparatus and oedometer.
-
Determination of changes in viscosity of hydrogel depending on shear rate (1.1 to 55 s-1).
Dane BadawczeThe rheological characteristics of hydrogel were made on the basis of a viscosity measurement using a Brookfield viscometer, using LV SC4 - 25 spindle and shear rates from 1.1 to 55 s-1.
-
Determination of changes in viscosity of refined oil depending on the temperature (19-96 Celsius degrees).
Dane BadawczeThe rheological characteristics of the refined oil were made on the basis of the viscosity assessment using a Brookfield viscometer with an LV SC4 - 18 spindle and a shear rate of 52.8 s-1 in from temperature 19-96 °C.
-
Determination of changes in viscosity of hydrogel depending on shear rate (1.7 to 34 s-1).
Dane BadawczeThe rheological characteristics of hydrogel were made on the basis of a viscosity measurement using a Brookfield viscometer, using LV SC4 - 27 spindle and shear rates from 1.7 to 34 s-1.
-
Determination of changes in viscosity of poly(acrylic acid) PAA solutions depending on shear rate.
Dane BadawczeThe rheological characteristics of poly(acrylic acid) PAA solutions were based on viscosity measurements using a Brookfield viscometer, using LV SC4 - 27 spindles and shear rates from 1,7 to 39 s-1 (Fig. 1). PAA solutions with were prepared in water. The data allowed to characterize the used PAA and assess their functional parameters as rheology modifying...
-
Determination of changes in viscosity of pectin gel depending on shear rate (1.1 to 55 s-1).
Dane BadawczeThe rheological characteristic of pectin gel (with concetration 0,45% m/m, in three independent repetition of sample) was made on the basis of a viscosity measurement using a Brookfield viscometer, using LV SC4 - 25 spindle and shear rates from 1.1 to 55 s-1.The data allowed to characterize the used hydrogel preparations and assess their functional...
-
Determination of changes in viscosity of high-fructose syrup stability of pectin hydrogels depending on the temperature (25-96 Celsius degrees).
Dane BadawczeThe rheological characteristics of the high-fructose syrup modified stability of pectin (added in a concentration 2% m/m) were made on the basis of the viscosity assessment using a Brookfield viscometer with an LV SC4 - 25 spindle and a shear rate of 0,22 s-1 in the temperature range 25-96 ° C. The data allowed selection of optimal conditions for the...
-
The effect of changes in the concentration of hydroxypropylcellulose on the rheological stability of pectin hydrogels.
Dane BadawczeThe rheological characteristics of the pectin hydrogel modified by hydroxypropylcellulose (added in a concetration range from 0.1 to 0.55% m/m) were made on the basis of the viscosity assessment using a Brookfield viscometer with an LV SC4 - 25 spindle and a shear rate of 0,22 s-1 in the temperature range 19-96 ° C.The data allowed selection of optimal...
-
Determination of changes in viscosity of pectin gel depending on shear rate (1.7 to 85 s-1).
Dane BadawczeThe rheological characteristic of pectin gel (with concetration 0,25% m/m, in two independent repetitions) wasmade on the basis of a viscosity measurement using a Brookfield viscometer, using LV SC4 - 27 spindle and shear rates from 1.7 to 85 s-1, in temperature of 25 C degee .The data allowed to characterize the used hydrogel preparations and assess...
-
Determination of changes in viscosity of chitosan solutions depending on shear rate.
Dane BadawczeThe rheological characteristics of chitosan solutions were based on viscosity measurements using a Brookfield viscometer, using LV SC4 - 25 spindles and shear rates from 4 to 53 s-1 (Fig. 1). Chitosan solutions with different molecular weights (low, medium and high) were prepared in concentrations from 1.5 to 3.0% in 0.5M acetic acid. The data allowed...
-
Determination of viscosity changes of protein hydrolyzate solutions depending on shear rate
Dane BadawczeRheological characteristics of connective tissue protein solutions were made on the basis of viscosity measurement using a Brookfield viscometer using LV SC4 - 27 spindles and shear rate of 85 s-1 (Fig. 1). Solutions of protein hydrolysates with a concentration of 2% in 0.5M acetic acid were prepared.
-
Determination of changes in viscosity of chitosan cosmetic preparations depending on shear rate.
Dane BadawczeThe rheological characteristics of chitosan were made on the basis of a viscosity measurement using a Brookfield viscometer, using LV SC4 - 25 spindles and shear rates from 0.3 to 32 s-1 (Fig. 1). Chitosan solutions at 1% concentrations in acetic acid were prepared. The samples were subjected to storage tests.
-
Determination of viscosity changes in dietary supplement solutions depending on temperature.
Dane BadawczeThe rheological characteristics of dietary supplement solutions were made based on viscosity measurement using a Brookfield viscometer, using the LV SC4 - 18 spindle and a shear rate of 53 s-1 (Fig.1).
-
Determination of denaturation temperature of connective tissue proteins by viscometric measurements.
Dane BadawczeViscometric denaturation temperature of connective tissue proteins was determined by measuring viscosity with a Brookfield viscometer, using a LV SC4 - 18, 25 or LV3 spindle and shear rates from 50 to 110 s-1 (Fig.1). Freeze-dried protein samples were dissolved in 0.5 M acetic acid at 4 °C and concentration of 20 mg/mL. The solution was stirred with...
-
Fresh properties of concrete mixes M0-M100 concrete mixes
Dane BadawczeDataset of fresh properties of concretes containing different amount of magnetite aggregate (M0-M100) mixes.*. ODS - open-source spreadsheet file file consists results of:
-
Finite element models used in diagnostics of transverse cracks in bridge approach pavement
Dane BadawczeTransverse cracks in the asphalt pavement were observed on bridge structures next to single-module expansion joints with a 5 meter approach slab set at the depth of 1 m. The finite element (FE) models of the approach pavement were created to investigate the reasons of premature cracking and crack initiation mechanism over the back edge of the abutment...
-
AeroSense Measurements: Wind Tunnel Ecole Centrale Lyon
Dane BadawczeData from wind tunnel tests of Aerosesne measurement system installed on NACA 63418 aerfoil in the anechoic wind tunnel at the Ecole Centrale Lyon.
-
Measurements of ultrasonic bulk and guided wave propagation in additively manufactured cubes and plates obtained by ultrasonic pulse velocity analyzer and scanning laser vibrometry
Dane BadawczeThe DataSet contains the results of measurements of ultrasonic wave propagation in additively manufactured samples made of polylactic acid (PLA). Three types of raster angles in two consecutive layers were assumed: 0°/90° (#1), 45°/-45° (#2) and 90°/90° (#3) with respect to the x-axis. For each printing variants a cubic sample (#C1-3) with dimensions...