Luminescence properties of TeOx thin films annealing under an oxidizing atmosphere
Open Research DataThe DataSet contains the emission and excitation spectra of TeOx thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. The sol was obtained by vigorously stirring precursor solution at 50°C for 2h, then the temperature was raised...
-
XRD patterns of VO2 and V2O3 thin films obtained at 500°C
Open Research DataThe DataSet contains the XRD patterns of VO2 and V2O3 thin films obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (3-9 AsP layers) were deposited on a silicon substrate and were annealing at 500°C under an argon atmosphere.
-
XRD patterns of VO2 and V2O3 thin films obtained at 700°C
Open Research DataThe DataSet contains the XRD patterns of VO2 and V2O3 thin films obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (5-9 AsP layers) were deposited on a silicon substrate and were annealing at 700°C under an argon atmosphere.
-
TEM and EDX study of the Al2O3 ultra thin films
Open Research DataThe ultra-thin layers of Al2O3 were deposited on a silicon substrates. The method of atomic layer deposition (Beneq TFS 200 ALD system) was chosen as the proper method of dielectric layer deposition. This method provides precise thickness control down to a single atomic layer. The precursors used were trimethylaluminum (Sigma-Aldrich) and purified water....
-
Optical measurements of lithium titanate sol-gel derived thin films
Open Research DataNanocrystalline thin films with 800 nm thickness were prepared by sol–gel method. To examine the influence of the annealing time on as-prepared films crystallization, the coatings were heated at 550 °C for 10, 20 and 80 h. On the basis of transmission characteristic optical properties were calculated. It was found that transmission through the thin...
-
SEM micrographs of morphology evolution of V2O5 thin films on quartz glass
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin films deposited on a quartz glass substrate. The as-prepared thin films were annealing under an oxidizing atmosphere in the temperature range 200-600C. The results show that the morphology of the films dependent on the annealing temperature.
-
SEM micrographs of morphology evolution of V2O5 thin films on silicon substrate
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin films deposited on a silicon substrate. The as-prepared thin films were annealing under an oxidizing atmosphere in the temperature range 250-600C. The results show that the morphology of the films dependent on the annealing temperature.
-
Structural investigations of the Al2O3 ultra thin films
Open Research DataUltra-thin layers of Al2O3 were deposited by atomic layer deposition (ALD) (Beneq TFS 200 ALD system). This method provides precise thickness control down to a single atomic layer. The precursors used were trimethylaluminum (Sigma-Aldrich) and purified water. The deposition of the atomic layer was carried out at 200 °C. Samples with a thickness of 2...
-
Luminescence properties of TeOx-Dy thin films annealing under an oxidizing atmosphere
Open Research DataThe DataSet contains the emission and excitation spectra of TeOx-Dy thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of dysprosium ions were added, the nitrates were used as a source of rare-earth ions....
-
Luminescence properties of TeOx-Tb thin films annealing under an oxidizing atmosphere
Open Research DataThe DataSet contains the emission and excitation spectra of TeOx-Tb thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of terbium ions were added, the nitrates were used as a source of rare-earth ions. The...
-
Luminescence properties of TeOx-Eu thin films annealing under an oxidizing atmosphere
Open Research DataThe DataSet contains the emission and excitation spectra of TeOx-Eu thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of europium ions were added, the nitrates were used as a source of rare-earth ions. The...
-
Impedance spectroscopy of the lithium titanate doped by copper thin films
Open Research DataLithium titanate doped by copper thin films were derived by sol-gel method. Prepared gel was deposited by spin-coating technique. Samples with various content of Cu were measured by impedance spectroscopy method in a wide range of temperature, from -120 up to 150 deg.
-
Optical measurements of LTO:Cu sol-gel derived thin films
Open Research DataLithium titanate doped by copper thin films were manufactured by chemical, sol-gel method. Flms were deposited on a Corning glass substrated by spin coater. To calculated optical band gap and other optcal parameters, UV-VIS spectroscopy measurements were performed. For measurements selected samples with various content of Cu.
-
XRD patterns of V2O5 thin films deposited on isotropic etching silicon substrates (111)
Open Research DataThe DataSet contains the XRD patterns of V2O5 thin films deposited on isotropic etching silicon substrates (111). The silicon wafers were etched in a mixture of nitric acid, hydrofluoric acid, and acetic acid in the ratio of 40:1:15. The soaking time for the substrates was from 30 to 90 seconds. The thin films were obtained by the sol-gel method. ...
-
SEM micrographs of V2O5 thin films deposited on isotropic etching silicon substrates (111)
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin films deposited on isotropic etching silicon substrates (111). The silicon wafers were etched in a mixture of nitric acid, hydrofluoric acid, and acetic acid in the ratio of 40:1:15. The soaking time for the substrates was from 30 to 90 seconds. The thin films were...
-
Chemical investigation of the Al2O3 ultra-thin films
Open Research DataUltra-thin layers of oluminum oxide (Al2O3) were deposited by ALD method. Atomic layer deposition provides precise thickness control down to a single atomic layer. The precursors used were trimethylaluminum (Sigma-Aldrich) and purified water. The deposition of the atomic layer was carried out at 200 °C. Samples with a thickness of 2 and 8 nm of alumina...
-
SEM micrographs of morphology evolution of VO2 and V2O3 thin films obtained at 1000°C
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of VO2 and V2O3 thin films obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films were deposited on a silicon and quartz glass substrate and were annealing at 1000°C under an argon atmosphere.
-
SEM micrographs of morphology evolution of VO2 and V2O3 thin films obtained at 700°C
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of VO2 and V2O3 thin films obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (3-9 AsP layers) were deposited on a silicon substrate and were annealing at 700°C under an argon...
-
SEM micrographs of morphology evolution of VO2 and V2O3 thin films obtained at 500°C
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of VO2 and V2O3 thin films obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (3-9 AsP layers) were deposited on a silicon substrate and were annealing at 500°C under an argon...
-
Luminescence properties of TeOx-2%Eu1.5%Tb1.5%Dy thin films annealing under an oxidizing atmosphere
Open Research DataThe DataSet contains the emission and excitation spectra of TeOx-2%Eu1.5%Tb1.5%Dy thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of rare-earth ions were added, the nitrates were used as a source of rare-earth...
-
Luminescence properties of TeOx-2%Eu1.5%Tb1.5%Tm thin films annealing under an oxidizing atmosphere
Open Research DataThe DataSet contains the emission and excitation spectra of TeOx-2%Eu1.5%Tb1.5%Tm thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of rare-earth ions were added, the nitrates were used as a source of rare-earth...
-
Luminescence properties of TeOx-1%Eu1.5%Tb2.5%Dy thin films annealing under an oxidizing atmosphere
Open Research DataThe DataSet contains the emission and excitation spectra of TeOx-1%Eu1.5%Tb2.5%Dy thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of rare-earth ions were added, the nitrates were used as a source of rare-earth...
-
Structure evolution of V2O5 thin films deposited on silicon substrate - High-Temperature X-ray Diffraction
Open Research DataThe DataSet contains the XRD patterns of V2O5 thin films deposited on silicon substrates (111). The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on the silicon substrate. The structure was measured in-situ during heating between 50-800°C under...
-
Structure and optical measurements of Eu doped tellurium oxide thin films
Open Research DataThin films were deposited by magnetron sputtering method and simultaneously heated at 200 oC. Presence of Eu ions and their valence states was confirmed by X-ray photoemission spectroscopy measurements. The structure of the films as well as the influence of europium dopant on crystalline structure of the films was examined by X-ray diffraction method. ...
-
Structure evolution of V2O5 thin films deposited on quartz glass substrate - High-Temperature X-ray Diffraction
Open Research DataThe DataSet contains the XRD patterns of V2O5 thin films deposited on guartz glass. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on the quartz glass substrate. The structure was measured in-situ during heating between 50-800°C under synthetic...
-
XPS data of as-grown BDD, as-implanted Mn-BDD, and annealed Mn-BDD thin films
Open Research DataXPS survey spectra and detailed spectra O1, C1s and Mn2p of as-grown BDD, as-implanted Mn-BDD, and annealed Mn-BDD thin films. X-ray photoelectron spectroscopy (XPS) studies were conducted on an Escalab 250 Xi from Thermo Fisher Scientific with an Al Kα radiation. Results were published in the paper ( https://doi.org/10.1002/adfm.202308617)
-
Graphene oxide thin films deposited on a PCB board - chemical analysis
Open Research DataGraphene oxides based films were measured by X-ray photoemission spectroscopy (XPS) method. TheXPS measurements were carried out with the Omicron NanoTechnology UHV equipment. The hemispherical spectrophotometer was equipped with a 128-channel collector. The XPS measurements were performed at room temperature at a pressure below 1.1 × 10−8 mBar. The...
-
Substrate characterization in a electrochemically derived Manganium-Cobaltium thin films
Open Research DataManganium-Cobaltium thin films were electrochemically deposited on a Ni foams subsrates in a one-step process at −1.1 V vs. Ag/AgCl in an aqueous solution of differently concentrated Mn(NO3)2·4H2O and Co(NO3)2·6H2O with the deposition time limited by charges of 60, 120, and 200 mC at 25 °C. The concentration ratios of Mn(NO3)2·4H2O to Co(NO3)2·6H2O...
-
The assessment of microbiological antimicrobial properties of PE film loaded with nanozinc filler
Open Research DataThe dataset contains the results of a single series of determinations of the antimicrobial properties against E. coli and S. aureus of polyethylene films containing the nanozinc filler.
-
Structural investigations of the LTO:Cu thin films
Open Research DataLithium titanate (Li1+xTi2-xO4) doped with Cu2+ ions was synthesized by sol-gel processing method. The structure was characterized by X-ray Diffraction (XRD). All samples revealed presence of LTO spinel phase. X-ray pattern of undoped LTO was free of any impurities and other crystal phases. Similarly, samples with low amount of copper dopant (x = 0.05...
-
The electrochemical studies of thin boron-doped diamond films deposited at conductive poly(lactic acid) 3D prints
Open Research DataThe dataset contains the electrochemical characteristics of the electrodes composed of thin boron-doped diamond films coated on commercially available graphene-doped polylactide acid. The boron doping level expressed as the [B]/[C] ratio in the gas phase for these studies was 500 and 10,000 ppm.
-
Scanning electron microscopy (SEM) images of boron-doped diamond thin films at poly(lactic acid)
Open Research DataThe dataset contains the photos obtained by scanning electron microscope(SEM), revealing the surface morphology and cross-section of boron-doped diamond electrodes on commercially available graphene-doped polylactide acid. The boron doping level expressed as the [B]/[C] ratio in the gas phase for these studies was 500 and 10,000 ppm. The top views of...
-
Morphology of the gold nanoislands
Open Research DataDewetting of the thin metallic films leads to formation of an isolated islands. morphology of nanostructures was measured by SEM microscope. Thin gold films with a thickness of 1.2 nm, 1.5 nm and 3.4 nm were anealed at 550, 600 and 650 Celcius degress.
-
Absorption and fluorescence spectra of 1,8-diazafluoren-9-one (DFO) in PVA polymer for different concentrations
Open Research DataAbsorption and fluorescence spectra of 1,8-diazafluoren-9-one (DFO) in PVA film for different concentrations of dye.
-
Chemical investigations of the MoO3 doped by K films deposited FTO
Open Research DataMoO3 thin films were synthesized via thermal annealing of thin, metallic Mo films deposited onto the FTO substrate using a magnetron sputtering system. The influence of photointercalation of alkali metal cation (K+) into the MoO3 structure on the photoelectrochemical properties of the molybdenum trioxide films was investigated. The chemical characterisation...
-
The AFM micrographs of V2O5 single crystals
Open Research DataThe DataSet contains the atomic force microscope images of the surface of V2O5 single crystals. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The As-prepared films were deposited on a quartz glass substrate and were annealing at 600°C under synthetic air.
-
XRD patterns of vanadium oxide nanostructures on silicon substrate obtained by V2O5 recrystallization
Open Research DataThe DataSet contains the XRD patterns of vanadium oxide nanostructures on silicon substrates obtained by recrystallization of V2O5 thin films between 800-1200°C under synthetic air. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials.
-
XRD patterns of vanadium oxide nanostructures on quartz glass substrate obtained by V2O5 recrystallization
Open Research DataThe DataSet contains the XRD patterns of vanadium oxide nanostructures on quartz glass substrates obtained by recrystallization of V2O5 thin films between 800-1200°C under synthetic air. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials.
-
Chemical composition of V2O5 nanorods
Open Research DataThe DataSet contains the chemical compositions of the V2O5 nanorods on a silicon substrate. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The As-prepared thin films were annealed at 600C under a synthetic air atmosphere.
-
SEM micrographs of vanadium oxide nanostructures obtained by V2O5 recrystallization at 1000°C
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of vanadium oxide nanostructures on quartz glass and silicon substrates obtained by recrystallization of V2O5 thin films at 1000°C under synthetic air. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials.
-
SEM micrographs of vanadium oxide nanostructures obtained by V2O5 recrystallization at 800°C
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of vanadium oxide nanostructures on quartz glass and silicon substrates obtained by recrystallization of V2O5 thin films at 800°C under synthetic air. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials.
-
SEM micrographs of vanadium oxide nanostructures obtained by V2O5 recrystallization at 1200°C
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of vanadium oxide nanostructures on quartz glass and silicon substrates obtained by recrystallization of V2O5 thin films at 1200°C under synthetic air. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials.
-
Spectroscopy properties of 1,8-diazafluoren-9-one (DFO) in PVA polymer for different concentrations
Open Research DataSpectroscopy properties: absorption and fluorescence spectra of 1,8-diazafluoren-9-one (DFO) in PVA film for different concentrations of dye.
-
Measurements of AuAg nanostructures
Open Research DataExtensive UV-vis measurements of AuAg alloyed nanostructures created from thin films. Plasmonic band position dependence on fabrication parameters.
-
Processed measurements of AuAg nanostructures
Open Research DataExtensive processed UV-vis measurements of AuAg alloyed nanostructures created from thin films. Plasmonic band position dependence on fabrication parameters.
-
UV-Vis measurements and SEM images of Ag nanostructures
Open Research DataUv-vis and SEM of Ag nanostructures. Structures were obtained by dewetting thin films. Various fabrication conditions i.e. temperature, time of the annealing and thickness of the initial layer were subsequently changed.
-
SEM - Expanded polystyrene coated by TiO2 or SiO2-TiO2
Open Research DataData contain SEM images taken in SEM Hitachi SU8000 with voltage of 5.0 kV. SEM images show expanded plystyrene spheres coated by a thin layer of TiO2 or bilayer SiO2-TiO2.
-
Raw data of AuAg nanoalloy plasmon resonances used for machine learning method
Open Research DataRaw data used for machine learning process. UV-vis measurements of AuAg alloyed nanostructures created from thin films. Plasmonic band position dependence on fabrication parameters. Small presentation reviewing achieved structures and their properties.
-
TEM imaging of metal nanoparticle cross section
Open Research DataTEM microscope was used for a imaging of metallic nanostructures. Metallic nanostructures were manufactured by thermal annealing of thin films. Gold and silver nanostructures were chosen for measurements. Samples were annealed for 15 and 60 minutes at 550 deg.
-
SEM analysis of the TiO2 layers deposited on a FTO substrates
Open Research DataTitanium dioxide layers were deposited on a FTO conducting glass by sol-gel method. For sol gel synthesis butoxy titanium and ethanol were used as a reagents. Samples were sintered in a furnace at temperature of 600 deg. SEM measurements were performed by FEI Quanta FEG250 microscope. SEM images of a cross-section of samples exhibit a porous structures...