DLC coating doped with W in ring-on-ring sliding with saline solution (0.9% wt.) lubrication 10MPa/0.1m/s
Dane BadawczeWear tests in sliding friction of 1% W (tungsten) doped DLC coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, DLC-W over DLC-W. Mean contact stress: 10MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: SALINE SOLUTION (0.9% wt.). Tribometer: PT-3. Overall test time >15h....
-
Detection of the acoustic interferences during AFM operation
Dane BadawczeAtomic force microscopy is a particularly complicated surface imaging technique due to the large number of factors that affect the quality of the resulting images. They are obviously difficult and sometimes even impossible to control at the same time. One of such factors may even be the seismological location of the building or the influence of mechanical...
-
Examples of AFM applications in liquid environment
Dane BadawczeImportant advantage of atomic force microscopy (also tunneling microscopy) is the ability to work in different environments (vacuum, controlled atmosphere, liquid environment). The last one, open interesting possibilities, such as imaging of delicate biological materials in their natural state. The use of electrochemical mode allows for the modification...
-
Split-beam echosounder data from Gdansk Deep Summer 2019
Dane BadawczeThe acoustic data was collected in 2019, in the Gdansk Deep, in the season: Summer. Data was collected during the day and night. Three split-beam echosounders with frequencies of 38 kHz, 120 kHz and 333 kHz were used to collect the data. The data was collected while the ship was sailing. To ensure data quality, echosounders were calibrated and passive...
-
Ambient vibrations - footbridge over the Kolibkowski Stream in Gdynia, span P2
Dane BadawczeAmbient vibration tests carried out on the P2 span of the footbridge over the Kolibkowski Stream. The research was carried out using a set of 14 acceleration sensors - MEMS accelerometers TE 4332M3-002 and TE 4312M3-002, which allowed for simultaneous measurement and recording of 20 acceleration channels. These sensors are characterized by a natural...
-
Ambient vibrations - footbridge over the Kolibkowski Stream in Gdynia, span P3
Dane BadawczeAmbient vibration tests carried out on the P3 span of the footbridge over the Kolibkowski Stream. The research was carried out using a set of 14 acceleration sensors - MEMS accelerometers TE 4332M3-002 and TE 4312M3-002, which allowed for simultaneous measurement and recording of 20 acceleration channels. These sensors are characterized by a natural...
-
Split-beam echosounder data from Puck Bay autumn 2018
Dane BadawczeThe acoustic data was collected in 2018, in the Bay of Puck, in the seasons: autumn. Data was collected during the day and night. Three split-beam echosounders with frequencies of 38 kHz, 120 kHz and 333 kHz were used to collect the data. The data was collected at a designated study area not far from the city of Hel, while the ship was sailing. To ensure...
-
Split-beam echosounder data from Puck Bay spring 2019
Dane BadawczeThe acoustic data was collected in 2019, in the Bay of Puck, in the season: spring. Data was collected during the day and night. Three split-beam echosounders with frequencies of 38 kHz, 120 kHz and 333 kHz were used to collect the data. The data was collected at a designated study area not far from the city of Hel, while the ship was sailing. To ensure...
-
Split-beam echosounder data from Puck Bay spring 2019 Part II
Dane BadawczeThe acoustic data was collected in 2019, in the Bay of Puck, in the season: spring. Data was collected during the sunrise and sunset. Three split-beam echosounders with frequencies of 38 kHz, 120 kHz and 333 kHz were used to collect the data. The data was collected at a designated study area not far from the city of Hel, while the ship was sailing....
-
LDRAW based positional renders of LEGO bricks
Dane Badawcze243 different LEGO bricks renders of size 250x250 in 5 colors in 120 viewing angles stored as JPEG images. The renders are used to train neural networks for bricks recognition. All images were generated using L3P (http://www.hassings.dk/l3/l3p.html) and POV-Ray (http://www.povray.org/) tools and were based on the 3D models from LDraw (https://www.ldraw.org/)...
-
The AC motor voltage and audible noise waveforms in ship’s electrical drive systems with frequency converters
Dane BadawczeThe presented dataset is part of research focusing on the impact of the ship's electrical drive systems with frequency converters on vibrations and the level of audible noise on ships.
-
Split-beam echosounder data from Puck Bay winter 2019
Dane BadawczeThe acoustic data was collected in 2019, in the Bay of Puck, in the season: winter. Data was collected during the day and night. Three split-beam echosounders with frequencies of 38 kHz, 120 kHz and 333 kHz were used to collect the data. The data was collected at a designated study area not far from the city of Hel, on the route Hel - Gdynia and on...
-
Split-beam echosounder data from Puck Bay autumn 2018 Part II
Dane BadawczeThe acoustic data was collected in 2018, in the Bay of Puck, in the seasons: autumn. Data was collected during the day and night. Three split-beam echosounders with frequencies of 38 kHz, 120 kHz and 333 kHz were used to collect the data. The data was collected at a designated study area not far from the city of Hel and on the route Hel - Gdynia while...
-
The morphology of vanadate glasses containing BaTiO3 measured with the use of AFM
Dane BadawczeThe morphology of vanadate glasses doped with BaTiO3 was measured with the use of AFM method. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured...
-
The morphology of vanadate glass-ceramics containing BaTiO3 measured with the use of AFM
Dane BadawczeThe structure of vanadate glass-ceramics doped with BaTiO3 was measured by AFM technique. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on...
-
Linear impedance of Bi2VO5.5 glass-ceramic measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 glass-ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Effect of C-1748 derivatives on the biofilm formation of C. albicans ATCC 10231 cells
Dane BadawczeThe datasets contain the results of the impact of five C-1748 derivatives (IKE28 - IKE32) on the biofilm formation of Candida albicans strain ATCC 10231 cells. Photographic documentation prepared with the TECAN Spark 10M titration plate reader.
-
Effect of C-1748 derivatives on the morphological transformation of C. albicans ATCC 10231 cells
Dane BadawczeThe datasets contain the results of the impact of five C-1748 derivatives (IKE28 - IKE32) on morphological transformation of Candida albicans strain ATCC 10231 cells. Photographic documentation prepared with the TECAN Spark 10M titration plate reader.
-
The morphology of vanadate glasses containing BaTiO3
Dane BadawczeThe morphology of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573 K) brass...
-
The morphology of lead-borate glasses and nanocomposites doped with iron oxide
Dane BadawczeThe topography of iron-doped borate glasses and glass-ceramics were studied. Samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 < x < 37 in mol%) were prepared by the conventional meltquenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated (573 K) brass plate...
-
The topography of Bi2VO5.5 ceramics prepared by melt-quenching technique was measured with confocal microscope
Dane BadawczeThe topography of Bi2VO5.5 ceramics prepared by melt-quenching technique was measured by confocal microscope.
-
The structure of lead-borate glasses containing nanocrystallites of iron oxides
Dane BadawczeThe structure of iron-doped glasses and glass-ceramics were studied. Glass samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 b x b 37, in mol%) were prepared by the conventional melt quenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated (573 K) brass plate and...
-
Linear impedance of strontium–borate glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of strontium–borate glass was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 glass-ceramic annealed at 423 K measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 glass-ceramic annealed at 423 K prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Effect of novel bisacridines (IKE16, IKE18, IKE19, IKE21) and IE10 on the biofilm formation of C. albicans ATCC 10231 cells
Dane BadawczeThe datasets contain the results of the impact of novel bisacridines (IKE16, IKE18, IKE19, IKE21) and IE10 on the biofilm formation of Candida albicans strain ATCC 10231 cells. Photographic documentation prepared with the TECAN Spark 10M titration plate reader.
-
Simulation of the weight averaging of pulse frequency modulated sensor output signal
Dane BadawczeThe aim of the research is investigation of the efficiency of weight averaging of pulse frequency modulated signal. It was shown that from the point of view of the reduction of the sampling error the best are polynomial weighing functions, for which the maximum of this component error decreases proportionally to the appropriate power of the number of...
-
The structure of vanadate glass-ceramics containing BaTiO3 measured with X-ray diffraction method
Dane BadawczeThe structure of vanadate glass-ceramics doped with BaTiO3 was measured by XRD. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated...
-
Correction of far-field measurements obtained in non-anechoic test site
Dane BadawczeThe dataset contains raw and processed measurements of radiation pattern characteristics performed in non-anechoic regime for two geometrically small antenna structures: a spline-parameterized Vivaldi structure and a compact spline-based monopole. The responses have been obtained at the selected frequencies of interest as a function of mentioned structures...
-
Linear impedance of vanadate glasses containing BaTiO3
Dane BadawczeThe linear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
The morphology of vanadate glass-ceramics containing BaTiO3
Dane BadawczeThe morphology of vanadate glass-ceramic doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
Topography of barium-vanadate glasses
Dane BadawczeThe topography of barium-vanadate glasses was measured. Samples of the composition of xBaO-(100-x)V2O5 where x= 30, 40 and 45 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents: BaO (≥99.9%, P.P.H STANLAB Sp.J.) and V2O5 (≥99.9%, POCH) were thoroughly mixed in an agate mortar. The melting was performed...
-
Measurements of electrically small antenna radiation patterns in non-anechoic environments using TGM
Dane BadawczeThe dataset contains raw and processed measurements of radiation pattern characteristics performed in non-anechoic regime for four antenna structures: a spline-parameterized Vivaldi structure, a compact spline-based monopole, super-ultrawideband antenna, and a quasi-Yagi component. The responses have been obtained at the selected frequencies of interest...
-
Linear impedance of strontium–borate glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of strontium–borate glass was measured by impedance spectroscopy method.
-
Electrical properties of lead-borate glasses and glass-ceramics containing iron ions
Dane BadawczeElectrical properties were studied for borate-lead glasses and glass-ceramics doped with iron ions. Glass samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 b x b 37, in mol%) were prepared by the conventional melt quenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated...
-
Dielectric properties of barium-vanadate glasses
Dane BadawczeThe linear impedance of barium-vanadate glasses was measured. Samples of the composition of xBaO-(100-x)V2O5 where x= 30, 40 and 45 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents: BaO (≥99.9%, P.P.H STANLAB Sp.J.) and V2O5 (≥99.9%, POCH) were thoroughly mixed in an agate mortar. The melting was...
-
The structure of vanadate glasses containing BaTiO3.
Dane BadawczeThe structure of vanadate glasses doped with BaTiO3 was measured by SEM technique. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated...
-
Linear impedance of vanadate glass-ceramics containing BaTiO3
Dane BadawczeThe linear impedance of vanadate glass-ceramics containing BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated...
-
The topography of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses measured with confocal microscope
Dane BadawczeThe topography of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses measured with confocal microscope.
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method
Dane BadawczeThe linear electrcial properties as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
The structure of 50(2Bi2O3-V2O5)-50SrB4O7 measured with X-ray diffraction method during heating
Dane BadawczeThe structure changes of 50(2Bi2O3-V2O5)-50SrB4O7 glass occurred during increase in temperature was measured by XRD.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
The morphology of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses measured with AFM
Dane BadawczeThe morphology of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses was measured with the use of atomic force microscope.
-
Magnetic flux leakage signals of near side defects measured with different velocities
Dane BadawczeThe dataset contains raw signals measured with the use of the magnetic flux leakage (MFL) technique. Linear Hall effect sensors A1324 were used to measure magnetic flux leakage. Three voltage signals were measured: Bx sensor output, Bz1 sensor output, and difference of Bz1 and Bz2 outputs. An output of a Bx sensor was directly proportional to the tangential...
-
Magnetic flux leakage signals of far side defects measured with different velocities
Dane BadawczeThe dataset contains raw signals measured with the use of the magnetic flux leakage (MFL) technique. Linear Hall effect sensors A1324 were used to measure magnetic flux leakage. Three voltage signals were measured: Bx sensor output, Bz1 sensor output, and difference of Bz1 and Bz2 outputs. An output of a Bx sensor was directly proportional to the tangential...
-
Measurements of guided wave propagation in CFRP/steel adhesive joints obtained by scanning laser vibrometry
Dane BadawczeThe DataSet contains guided wave signals measured in adhesive joints of steel plates (steel of type S355 with a thickness of 11.9 mm ) and carbon fibre reinforced polymer (CarboDur S1012 with a thickness of 1.24 mm). The samples were as follows: #0 – intact; #1 – 10% disbond; #2 – 20% disbond; #3 – 50% disbond; #4 – 80% disbond; #5 – 100% disbond.
-
The structure of vanadate glass-ceramics containing BaTiO3.
Dane BadawczeThe structure of vanadate glass-ceramics doped with BaTiO3 was measured by SEM technique. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on...
-
Topography of iron-phosphate glasses doped with niobium and titanium tested by confocal microscope
Dane BadawczeThe topography of phosphate-iron glasses containing niobium and titanium were investigated with the use of confocal miscroscope. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5, 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 and 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents...