Filters
total: 623
filtered: 64
Chosen catalog filters
Search results for: SURFACE MORPHOLOGY
-
SEM micrographs of morphology evolution of V2O5 nanostructures
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of morphology evolution of vanadium pentaoxide nanostructures obtained by the sol-gel, depending on annealing temperature under synthetic air. The results show that the morphology dependent on the annealing temperature.
-
Scanning electron microscopy (SEM) images of the boron-dopied diamond surfaces
Open Research DataThe dataset contains the scanning electron micrographs (SEM), revealing the surface morphology of diamond electrodes on different substrates. The diamond surface is characterized by an aggregation of crystals that do not form a continuous layer.
-
Scanning electron microscopy (SEM) images of the boron-dopied diamond surfaces
Open Research DataThe dataset contains the scanning electron micrographs (SEM), revealing the surface morphology of diamond electrodes on silicon substrates. The diamond surface is characterized by ultra-crystalline diamonds obtained by CVD synthesis.
-
SEM micrographs of V2O5 thin film morphology dependent on substrate types
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin film morphology dependent on substrate types. The as-prepared thin films were deposited on alumina, zirconium, zirconium oxide and metallic vanadium substrate, then was annealing under an oxidizing atmosphere at 600C for 10h. The results show that the morphology of...
-
Scanning electron microscopy (SEM) images of the boron-doped carbon nanowalls surfaces
Open Research DataThe dataset contains the scanning electron micrographs (SEM), revealing the surface morphology of boron-doped carbon nanowalls electrodes on silicon substrates. The surface is characterized by nano-walled structures. The obtained electrodes were doped with boron at the level of [B]/[C] = 5000ppm in the gas atmosphere during the synthesis.
-
Scanning electron microscopy (SEM) images of the boron-dopied carbon nanowalls surfaces
Open Research DataThe dataset contains the scanning electron micrographs (SEM), revealing the surface morphology of boron-doped carbon nanowalls electrodes on silicon substrates. The surface is characterized by nano-walled structures. The obtained electrodes were doped with boron at the level of [B]/[C] = 1200ppm in the gas atmosphere during the synthesis.
-
Scanning electron microscopy (SEM) images of the boron-doped carbon nanowalls surfaces
Open Research DataThe dataset contains the scanning electron micrographs (SEM), revealing the surface morphology of boron-doped carbon nanowalls electrodes on silicon substrates. The surface is characterized by nano-walled structures. The obtained electrodes were doped with boron at the level of [B]/[C] = 2000ppm in the gas atmosphere during the synthesis.
-
SEM micrographs of morphology evolution of VO2 and V2O3 nanostructures
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of VO2 and V2O3 nanostructures obtained by the sol-gel with different reaction conditions. The information about xerogel powder synthesis is described in the Journal of Nanomaterials. The xerogel powder was annealing under argon atmosphere in the temperature range 400-800C. The...
-
SEM micrographs of morphology evolution of V2O3 nanostructures
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O3 nanostructures obtained by the sol-gel with different reaction conditions. The xerogel powder was annealing under a reducing atmosphere (94% Ar, 6% H2) in the temperature range 350-700C. The results show that the morphology dependent on the annealing temperature.
-
Temperature of formation of Au nanostructures
Open Research DataNanostructures were obtained via annealing of thin Au films. In order to determine possible nanoislands formation mechanisms, dependence on initial film thickness was examined. For the surface morphology studies, nanograin structure and chemical composition analysis, SEM, HR TEM and EDS measurements were performed, respectively. Morphology studies shown...
-
The AFM micrographs of vanadium oxides thin films deposited on silicon - the influence of the thickness of the film on morphology
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (1, 2 or 3 AsP layers) were deposited on a silicon substrate and were annealing...
-
SEM micrographs of morphology evolution of V2O5 thin films on quartz glass
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin films deposited on a quartz glass substrate. The as-prepared thin films were annealing under an oxidizing atmosphere in the temperature range 200-600C. The results show that the morphology of the films dependent on the annealing temperature.
-
SEM micrographs of morphology evolution of V2O5 thin films on silicon substrate
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin films deposited on a silicon substrate. The as-prepared thin films were annealing under an oxidizing atmosphere in the temperature range 250-600C. The results show that the morphology of the films dependent on the annealing temperature.
-
Scanning electron microscopy (SEM) images of boron-doped diamond thin films at poly(lactic acid)
Open Research DataThe dataset contains the photos obtained by scanning electron microscope(SEM), revealing the surface morphology and cross-section of boron-doped diamond electrodes on commercially available graphene-doped polylactide acid. The boron doping level expressed as the [B]/[C] ratio in the gas phase for these studies was 500 and 10,000 ppm. The top views of...
-
The AFM micrographs of vanadium oxides thin films deposited on quartz glass - the influence of the thickness of the thin film on its morphology
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (1, 2 or 3 AsP layers) were deposited on a quartz glass substrate and were...
-
The AFM micrographs of V2O5 single crystals
Open Research DataThe DataSet contains the atomic force microscope images of the surface of V2O5 single crystals. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The As-prepared films were deposited on a quartz glass substrate and were annealing at 600°C under synthetic air.
-
The AFM micrographs of vanadium oxides thin films obtained at 800°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on a silicon substrate and vanadium thin films were obtained by annealing as-prepared films at...
-
The AFM micrographs of vanadium oxides thin films obtained at 1200°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 400°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 600°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of of vanadium oxides thin films obtained at 300°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxide thin films obtained at 100°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 150°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 200°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 450°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
SEM micrographs of NH4VO3 crystals - molar concetration factor after annealing
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of NH4VO3 nano_crystals obtained by the LPE-IonEx method with different morphology after annealing at 400C under argon atmosphere (with a heating rate of 10 C/min).
-
SEM micrographs of ammonium vanadate nanocrystals
Open Research DataThe DataSet contains the electron microscopy (SEM) micrographs of ammonium vanadate nanobelts obtained by the hydrothermal method with different conditions. The results show that the morphology of samples dependent on reaction conditions.
-
SEM micrographs of NH4VO3 crystals - molar concetration factor
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of NH4VO3 nano_crystals obtained by the LPE-IonEx method. The SEM images clearly show that the morphology of the end product can be nicely tuned by changing the molar concentration of ammonium salt in the solvent.
-
SEM micrographs of NH4VO3 crystals
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of NH4VO3 crystals obtained by the LPE-IonEx method. The SEM images clearly show that the morphology of the end product can be nicely tuned by changing the type of ammonium salt and the solvent. It can be concluded that the used solvent affected crystal shapes and their size was...
-
Morphology and structure of ammonium vanadates synthesis by hydrothermal method
Open Research DataThe DataSet contains the XRD patterns, FTIR spectra, and scanning electron microscopy (SEM) micrographs of ammonium vanadates synthesis by hydrothermal method from different NH4VO3 precursors. The results reveal that a mixture of (NH4)V4O10xH2O and(NH4)0.76V4O10 was obtained for both precursors, however the contribution of each phase was different for...
-
SEM images of dewetted gold films
Open Research DataGold nanostructures were prepared on silicon - Si(111) as a substrate. as a result of dewetting process. Thin golds films were deposited using a table-top dc magnetron sputtering coater under pure Ar plasma conditions . The Au target had 99.99% purity, the rate of Au layer deposition was about 0.4 nm·s−1 and the incident power was 32 W. The thickness...
-
SEM images of tge gold nanostructures on silicon
Open Research DataAu nanostructures were prepared on Si(111) as a substrate. The substrates (1 × 1 cm2 of area) were cleaned with acetylacetone and then rinsed in ethanol. Thin Au films (with thicknesses in a range of 1.7–5.0 nm) were deposited using a table-top dc magnetron sputtering coater (EM SCD 500, Leica) under pure Ar plasma conditions (Argon, Air Products 99.999%)....
-
Formation of gold anostructures detected by SEM microscope
Open Research DataGold nanostructures were prepared on silicon - Si(111) as a substrate. The substrates (1 × 1 cm2 of area) were cleaned with acetylacetone and then rinsed in ethanol. Thin Au films (with thicknesses in a range of 1.7–5.0 nm) were deposited using a table-top dc magnetron sputtering coater (EM SCD 500, Leica) under pure Ar plasma conditions (Argon, Air...
-
Exemplary AFM application in cosmetology
Open Research DataAtomic force microscopy can be used in the diagnosis of the condition of human tissues such as skin, nails and hair. This is obviously related to the use of a variety of cosmetic products and can be understood as an attempt to assess their long-term impact on human appearance and health. An example may be the studies presented in [1] indicating the...
-
Identification of intermetallic phases in the structure of austenitic steel with use of Scanning Kelvin Probe Microscopy
Open Research DataDelta ferrite is formed in austenitic steels during the solidification of the alloy and its welds. It can also occur as a stable phase in any temperature range in high-alloy austenitic-ferritic steels. Depending on the amount, it can change into gamma and sigma phases and into ferrite with variable chromium content. The main role of delta ferrite in...
-
Morphology and structure of V2O5 nanorods deposited on the silicon substrate after reduction
Open Research DataThe DataSet contains the XRD patterns and SEM micrographs of V2O5 nanorods on the silicon substrate after thermal treatment under a reducing atmosphere. Thin films were annealed at 500C for 40 under a reducing atmosphere (94% Ar, 6% H2).
-
SEM micrographs of morphology evolution of VO2 and V2O3 thin films obtained at 1000°C
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of VO2 and V2O3 thin films obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films were deposited on a silicon and quartz glass substrate and were annealing at 1000°C under an argon atmosphere.
-
SEM micrographs of morphology evolution of VO2 and V2O3 thin films obtained at 700°C
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of VO2 and V2O3 thin films obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (3-9 AsP layers) were deposited on a silicon substrate and were annealing at 700°C under an argon...
-
SEM micrographs of morphology evolution of VO2 and V2O3 thin films obtained at 500°C
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of VO2 and V2O3 thin films obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (3-9 AsP layers) were deposited on a silicon substrate and were annealing at 500°C under an argon...
-
The morphology of V2O5 nanostructures deposited on quartz glass
Open Research DataThe DataSet contains the confocal microscope images of morphology evolution of vanadium pentaoxide nanostructures on quartz glass obtained by annealing as-prepared films at 500C and 600C under synthetic air.
-
SEM micrographs of morphology evolution of VO2 and V2O3 thin films obtained at 1000°C dependent on film thickness
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of VO2 and V2O3 thin films obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (2-3 AsP layers) were deposited on a silicon substrate and were annealing at 1000°C under an argon...
-
The morphology of vanadate glasses containing BaTiO3
Open Research DataThe morphology of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573 K) brass...
-
Morphology of the gold nanoislands
Open Research DataDewetting of the thin metallic films leads to formation of an isolated islands. morphology of nanostructures was measured by SEM microscope. Thin gold films with a thickness of 1.2 nm, 1.5 nm and 3.4 nm were anealed at 550, 600 and 650 Celcius degress.
-
LIDAR data from a cliff measurement conducted in the vicinity of the town of Jastrzębia Góra on the Baltic Sea coast
Open Research DataMeasurement data were obtained during research related to the use of LiDAR observations to assess the stability of a coastal cliff. The collected information comes from measurements conducted in the vicinity of the town of Jastrzębia Góra on the Baltic Sea coast. The acquired point cloud constitutes a comprehensive set of data regarding the geometry...
-
TEM (transmission electron microscopy) images and elemental mapping EDX (energy dispersive X-ray spectroscopy) of bulk boron and borophene obtained during ball milling
Open Research DataThese data contain TEM (transmission electron microscopy) images with corresponding elemental mapping EDX of bulk boron and borophene flakes after the ball-milling process (450 rpm, 6 h, 1 g). The data were collected to investigate the structure and morphology of the materials.
-
The morphology of vanadate glass-ceramics containing BaTiO3
Open Research DataThe morphology of vanadate glass-ceramic doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
Morphology of the sol-gel derived LTO:Cu films
Open Research DataMorphology of the lithium titanate doped by Cu thin films were investigated by SEM microscope. Films were deposited by spin-coater from sol-gel derived sol. SEM images showed a high porous structure, tipaciall for sol-gel based films. For measurements samples with a various content of Cu were selected.
-
The AFM micrographs of isotropic etching silicon substrates (111)
Open Research DataThe DataSet contains the atomic force microscope images of isotropic etching silicon substrates (111). The silicon wafers were etched in a mixture of nitric acid, hydrofluoric acid, and acetic acid in the ratio of 40:1:15. The soaking time for the substrates was from 20 to 90 seconds
-
SEM and Raman studies B:CNWs and BDD electrode used for electrochemical paraquat determination
Open Research DataThe dataset contains the scanning electron micrographs (SEM) and Raman spectra of B:CNWs and BDD samples deposited by MW-PECVD. SEM was used to characterise the morphology of BDD and B:CNW. In contrast, RAMAN was used to reveal the main differences in the crystalline structure of BDD and B:CNWs.
-
SEM inwestigation of the silver nanostructures
Open Research DataSilver thin films with a thickness of 1nm, 3nm, 5nm, 7nm and 9nm were deposited by a table-top magnetron sputtering unit in a pure argon plasma from a high-purity silver target. Silicon wafers was used as a substrates. As-deposired films were annealed in Ar atmosphere at 550 Celsius degree for 15 minutes.As a result of annealing, Ag nanostructures formed...