Wyniki wyszukiwania dla: BISMUTH–TELLURIUM ALLOY
-
Biocompatibility and bioactivity of load-bearing metallic implants
PublikacjaThe main objective of here presented research is to develop the titanium (Ti) alloy base composite materials possessing better biocompatibility, longer lifetime and bioactivity behaviour for load-bearing implants, e.g. hip joint and knee joint endoprosthesis. The development of such materials is performed through: modeling the material behaviour in biological environment in long time and developing of new procedures for such evaluation;...
-
Effect of Bi2O3 Excess on Morphology and Structure of BiNbO4 Ceramics
PublikacjaGoal of the present research was to fabricate BiNbO4 ceramics from the mixture of powders by the solid state reaction route and pressureless sintering at various temperatures (TS =8700C and TS =9100C) and study microstructure, phase composition and crystalline structure of BiNbO4 ceramics. Four batches were fabricated and examined, namely the one fabricated from the stoichiometric mixture of reagent – grade oxide powders, viz....
-
Novel two-step synthesis method of thin film heterojunction of BiOBr/Bi2WO6 with improved visible-light-driven photocatalytic activity
PublikacjaA novel two-step ionic liquid assisted procedure was applied for a controllable synthesis of BiOBr/Bi2WO6 heterojunction thin films. The preparation route involved an anodic oxidation of tungsten foil and hydrothermal transformation of as-anodized oxide in the presence of bismuth precursor and ionic liquid, N-butylpyridinium bromide [BPy][Br]. The BiOBr plates with irregular shapes adhered to the surface of flower-like Bi2WO6 and...
-
Widening of the electroactivity potential range by composite formation – capacitive properties of TiO2/BiVO4/PEDOT:PSS electrodes in contact with an aqueous electrolyte
PublikacjaComposites based on the titania nanotubes were tested in aqueous electrolyte as a potential electrode material for energy storage devices. The nanotubular morphology of TiO2 was obtained by Ti anodization. TiO2 nanotubes were covered by a thin layer of bismuth vanadate using pulsed laser deposition. The formation of the TiO2/BiVO4 junction leads to enhancement of pseudocapacitance in the cathodic potential range. The third component,...
-
Materials Design for the Titanium Scaffold Based Implant
PublikacjaThe main objective of here presented research is a design the scaffold/porous titanium(Ti) alloy based composite material demonstrating better biocompatibility, longer lifetime andbioactivity behaviour for load-bearing implants. The development of such material is proposed bymaking a number of consecutive tasks. Modelling the mechanical, biomechanical and biologicalbehavior of porous titanium structure and an elaboration of results...
-
LCF behavior of 2024AA under uni- and biaxial loading taking into account creep pre-deformation
PublikacjaThis study presents the results of experimental low-cycle fatigue (LCF) tests of aluminum 2024 alloy T3511 temper in uni- and biaxial loading states. Tests were carried out on both the as-received material (hardened extruded rods) and material with different pre-deformation histories. These deformations were carried out in the creep process at 200 °C and 300 °C for two different levels of at each temperature. The pre-deformed material’s...
-
Materials Design for the Titanium Scaffold Based Implant
PublikacjaThe main objective of here presented research is a design the scaffold/porous titanium(Ti) alloy based composite material demonstrating better biocompatibility, longer lifetime andbioactivity behaviour for load-bearing implants. The development of such material is proposed bymaking a number of consecutive tasks. Modelling the mechanical, biomechanical and biologicalbehavior of porous titanium structure and an elaboration of results...
-
Effects of the preheating laser treatment on microstructure and corrosion resistance of Ti6Al4V bioalloy
PublikacjaThe laser remelting of the Ti6Al4V alloy was made on specimens pre-heated at elevated temperatures. The laser treatment effected in change of microstructures of surface layers and an appearance of blisters and numerous cracks. The corrosion tests demonstrated the decrease in corrosion resistance for each preheating temperature. The observed effects were attributed to negative influence of excessive compressive stresses with no...
-
Formation of Porous Structure of the Metallic Materials Used on Bone Implants
PublikacjaResearch on improvement of structure and fabrication methods of the bone implants are carried out for many years. Research are aimed to shape the structures, that will have a Young's modulus value similar to the value of the human bones Young's modulus. Depending on theporosity, Young's moduli can even be tailored to match the modulus of bone closer than solid metals can, thus reducing the problems associated with stress shielding...
-
Hydrogen Embrittlement and Oxide Layer E ect in the Cathodically Charged Zircaloy-2
PublikacjaThe present paper is aimed at determining the less investigated effects of hydrogen uptake on the microstructure and the mechanical behavior of the oxidized Zircaloy-2 alloy. The specimens were oxidized and charged with hydrogen. The different oxidation temperatures and cathodic current densities were applied. The scanning electron microscopy, X-ray electron diffraction spectroscopy, hydrogen absorption assessment, tensile, and...
-
Numerical and Analytical Investigation of Aluminium Bracket Strengthening
PublikacjaThis paper focuses on an analytical and numerical investigation of aluminium brackets used to fasten light-weight curtain walls to building facilities. The authors propose a solution to increase the load capacity of aluminium brackets by means of additional cover plates (straps). This paper also includes a short survey of literature and material properties concerning the EN AW-6060 T6 aluminium alloy. This paper suggests an initiation...
-
SEM micrographs of aluminium corrosion in alkaline media with various bee products as corrosion inhibitors
Dane BadawczeThis dataset contains various scanning electron microscopy (SEM) micrographs of AA5754 aluminum alloy samples exposed to the corrosive alkaline environment without and with the addition of various bee products to act as green corrosion inhibitors. The products are bee pollen, honey, and putty. They were investigated in bicarbonate buffer (pH =10 or...
-
The exemplary Kelvin probe microscopy studies of sensitized austenitic stainless steels
Dane BadawczeThe dataset summarizes the results of imaging the surface potential distribution using the Kelvin probe scanning technique. Due to the fact that the potential measured in this way is proportional to the electrochemical potential of metals or intermetallic phases, it is possible to assess the nobility differences of various alloy components. In the case...
-
Determination of causes of accelerated local corrosion of austenitic steels in water supply systems
PublikacjaThis paper concerns an inspection of a water supply system, made of AISI 304 steel, which showed signs of local corrosion at the weld. Such corrosion caused material perforation after very short periods of operation. It was revealed that steel was sensitised during the welding process. It was also proven that chromium micro-segregation occurred in the alloy leading to galvanic cell formation which initialised the process of pitting...
-
Some problems of slide bearing material fatigue evaluation.
PublikacjaA slide bearing alloy resistance against fatigue failures have been investigated for three different lubricants, different heat loadings and different stress ratio κ values. The research methods and data handling procedures for determination of particular parameter effects on fatigue strength have been described and analysed for experiments that were set and performed in laboratory tester SKMR-2. Main and interaction effects of...
-
Failure analysis of the exhaust valve face in diesel marine engine
PublikacjaThe exhaust valve from marine diesel engine which was damaged after 2000 hours of service was investigated. In order to prolong the service time the valve face was cladded with cobalt base alloy using laser technique. After failure microstructural and chemical analyses reviled that cladding process was conducted improperly. The chemical composition of the clad layer was far from the designed one and what more completely inhomogeneous....
-
Ultrafast high-temperature sintering (UHS) of cerium oxide-based compound
PublikacjaUltrafast high-temperature sintering (UHS) is an innovative sintering technique that can densify ceramics in a few seconds, dramatically reducing the carbon footprint and firing costs. In this work, the feasibility of applying UHS in Gd-doped ceria (GDC) and GDC-Er-stabilized bismuth oxide (ESB) composite powders was investigated. At high UHS currents (22-24 A), a fully dense GDC sample with a large grain size was obtained. Nonetheless,...
-
Influence of processing conditions on crystal structure of BiNbO 4 ceramics
PublikacjaBismuth niobate (BiNbO4) has attracted attention as a low-fired ceramics with promising microwave application potential. It belongs to the bismutocolumbite oxides with similarly to scheelite-like stibiotantalite structure (SbTaO4) A3+B5+O4. Aim of the present research was to fabricate BiNbO4 ceramics by solid state reaction route from the mixture of simple oxides viz. Bi2O3, and Nb2O5, and study its phase composition as well as...
-
Determination of ionic conductivity in the Bi-Si-O and Pb-Si-O glasses
PublikacjaImpedance spectroscopy measurements in various gas atmospheres were carried out in order to explain the doubts about the type of carriers and the mechanism of electrical conductivity in Bi-Si-O and Pb-Si-O glasses. In bismuth silicate glass, a typical ionic conductivity with oxygen ions as charge carriers was observed. The level of electrical conductivity of the glass at 400 °C was 5 × 10−8 S·cm−1 , with the activation energy of...
-
Glass-ceramic sealants and steel interconnects: accelerated interfacial stability and reactivity tests at high temperature
PublikacjaHigh-temperature reactions between glass-ceramic sealants and Fe-Cr alloy interconnects may lead to the formation of undesirable phases, and consequently degradation of solid oxide fuel/electrolyser devices. In this work, three different glass-ceramic sealants (Na-containing, Ba-containing, Sr-containing compositions) and Fe22Cr stainless steel powders (raw and pre-oxidised) are considered in order to test their chemical reactivity...
-
Vascular stents - materials and manufacturing technologies
PublikacjaThe objective of this article is to present materials and technology for the manufacture of vascular stents with appropriate design requirements. The use of the right material is very important in implantology. A biomaterial introduced into the circulatory system must be biocompatible and hemocompatible. At the same time, it should not initiate toxic, mutagenic, or immunological reactions. Currently, 316L stainless steel (316L...
-
Właściwości złączy różnoimiennych stopu niklu Incoloy 800H ze stalą odporną na korozję 316L
PublikacjaW artykule przedstawiono problemy związane z wykonywaniem połączeń różnoimiennych typu Incoloy 800HT – austenityczna stal odporna na korozję 316L. Wykonano badania nieniszczące oraz niszczące, których wyniki pozwoliły na weryfikacje jakości wykonanych złączy próbnych. Nie stwierdzono występowania niezgodności spawalniczych oraz uzyskano wysokie właściwości wytrzymałościowe złączy. Badania metalograficzne ujawniły poprawne struktury...
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 009_v_2
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 009_v_3
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 009_h_3
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 019_v_5
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 009_h_5
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 009_h_4
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 039_h_4
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 019_v_4
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 019_h_5
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 039_v_4
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 009_v_4
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 039_v_3
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 019_v_3
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 019_h_3
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 039_h_5
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 019_h_4
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 039_v_2
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 039_h_3
Dane BadawczeData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
Intergranular Corrosion Detection Using Electromagnetic Transducers for Ultrasonic Testing
PublikacjaThe aim of this paper is to create a research methodology that allows a quick analysis of the structural state of high alloy austenitic steels using non-destructive ultrasonic tests, in contrast to destructive standard methods. Electromagnetic acoustic transducers (EMAT) are used to generate and receive the ultrasonic wave and detect the microstructural changes caused by sample sensitization in elevated temperature, even after...
-
Environmental degradation of Ti alloys in artificial saliva and a role of fluorides
PublikacjaThe titanium and its alloys are potentially prone to hydrogen embrittlement, including those proposed for dental implants. The research has been aimed to assess a susceptibility to environment-enhanced degradation of the Ti-13Zr-13Nb alloy in artificial saliva with or without hydrofluoric acid, subject or not to cathodic polarisation. The results have shown that even if artificial saliva is safe environment, both cathodic polarization...
-
Cavitation Erosion of Nodular Cast Iron - Microstructural Effects
PublikacjaThe paper deals with susceptibility of nodular cast iron with ferritic-pearlitic matrix on cavitation erosion. Cavitation tests were carried out with the use of a cavitation erosion vibratory apparatus employing a vibration exciter operated at frequency of 20 kHz. The study allowed to determine the sequence of subsequent stages in which microstructure of cast iron in superficial regions is subject to degradation. The first features...
-
Investigation of corrosion behavior of 6060 and 6082 aluminum alloys under simulated acid rain conditions
PublikacjaInstantaneous impedance changes of 6060 and 6082 type aluminum alloys in pure water, and simulated acid rain poured into the pure water was investigated by dynamic electrochemical impedance spectroscopy (DEIS). In this way, the influence of aluminum content on the corrosion behavior of 6060 and 6082 type aluminum alloys immersed in simulated acid rain was determined. The corrosion rate of the alloy decreased with increasing Al...
-
Titania Nanofiber Scaffolds with Enhanced Biointegration Activity—Preliminary In Vitro Studies
PublikacjaThe increasing need for novel bone replacement materials has been driving numerous studies on modifying their surface to stimulate osteogenic cells expansion and to accelerate bone tissue regeneration. The goal of the presented study was to optimize the production of titania-based bioactive materials with high porosity and defined nanostructure, which supports the cell viability and growth. We have chosen to our experiments TiO2...
-
Thermal cooling process by nanofluid flowing near stagnating point of expanding surface under induced magnetism force: A computational case study
PublikacjaThis paper is dedicated to the exam of entropy age and research of the effect of mixing nanosolid additives over an extending sheet. In this review, Newtonian nanofluid version turned into researched at the actuated appealing field, heat radiation and variable heat conductivity results. With becoming modifications, the proven PDEs are moved into popular differential situations and paintings mathematically making use of a specific...
-
TiO 2 Co x O y composite nanotube arrays via one step electrochemical anodization for visible light–induced photocatalytic reaction
PublikacjaTiO2CoxOy (x = 1, y = 1 or x = 3, y = 4) composite photocatalysts have been synthesized via one step anodic anodization of TiCo alloys. The effects of the cobalt content in the alloy (5, 10 and 15 wt%), water content (2, 5 and 10%) in the electrolyte solution, and applied voltage (30, 40 and 50 V) during the anodization process on the morphology and surface properties. Additionally, the dependence of cobalt content in the nanotubes...
-
Nanostructure and dielectric behavior of vanadate glasses containing BaTiO3
PublikacjaThe ac and dc electrical conductivity of barium titanate doped bismuth-vanadate as-quenched and heat-treated materials was measured in the frequency range from 1 mHz to 1 MHz and in the temperature range from 153 K to 423 K with the impedance spectroscopy method. The microstructure was investigated by means of XRD, scanning electron microscopy (SEM), atomic force microscopy (AFM) and confocal microscopy. The obtained results showed...
-
Enhanced photoelectrochemical performance of inorganic-organic hybrid consisting of BiVO4 and PEDOT:PSS
PublikacjaThe PEDOT:PSS (poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate)) was electrodeposited on a thin layer of bismuth vanadate (BiVO 4 ) prepared using the pulsed laser deposition technique onto FTO. The inorganic-organic junction was characterized by Raman spectroscopy, UV-Vis spectroscopy and sc anning electron microscopy. Chronoamperometry curves, recorded under simulated solar light illumination,...
-
Highly Visible-Light-Photoactive Heterojunction Based on TiO2 Nanotubes Decorated by Pt Nanoparticles and Bi2S3 Quantum Dots
PublikacjaA heterojunction with excellent visible light response and stability based on titanium dioxide nanotubes (TiO2 NTs), bismuth sulfide quantum dots (Bi2S3 QDs), and platinum nanoparticles (Pt NPs) is proposed. Both Pt NPs (3.0 ± 0.2 nm) and Bi2S3 QDs (3.50 ± 0.20 nm) are well distributed on the (i) top parts, (ii) inner walls, and (iii) outer walls of the TiO2 NTs. Visible-light-induced photoreaction was initialized by excitation...