Results of nanoindentation test to calculate residual stress in an eyelet of undercarriage drag strut after laser treatment
Open Research DataIn order to determine the residual stress in the laser-processed an eyelet of undercarriage drag strut, a nanoindentation test was performed before and after stress relief annealing. For this purpose, after the hardness test, the sample was subjected to stress relief annealing at 270 °C for 2 hours. Annealing was performed in a vacuum furnace. Hardness...
-
Microstructure of cross-sections of samples after laser treatment for the article entitled "Mechanical and corrosive properties of Ti13Nb13Zr alloy subjected to laser treatment with MWCNTs coatings"
Open Research Data -
Impedance and cyclic voltammetry studies of GPLA electrodes after laser ablation
Open Research DataThe 3D printed GPLA electrodes present a brand new opportunity for electrode material for electrochemical biosensors. In order for the electrodes to be considered viable for electroanalysis studies, the pretreatment procedure must be applied in order to etch PLA matrix and reveal graphene filler. The following dataset presents an approach towards such...
-
Confocal microscopy analysis of DNA DSB in telomerase negative cells after exposure to TXT2 and TXT4
Open Research DataThe data sets contain confocal microscopic images showing the γ-H2AX with TRF2 after treatment of NHBE and U2OS cell lines with TXT2 and TXT4 in equitoxic concentrations. Images were acquired with an LSM 800 inverted laser scanning confocal microscope (Carl Zeiss; Dresden, Germany) equipped with an Airyscan detector using a ×63 1.4 NA Plan Apochromat...
-
Raman spectra and electrochemical data of carbon nanowall with tailored defects
Open Research DataThis dataset comprises of Raman spectra aquired with different excitation laser sources and the electrochemical data of defect-induced carbon nanowall electrodes (CNW).
-
Mechanical properties of single V2O5 nanocrystal - nanoindentation measurement in control of the max-load
Open Research DataThe DataSet contains the nanoindentation curves (indentation force Fn vs penetrationPd) for a single V2O5 nanocrystal supported on a substrate. The measurements were performed in control of the maximum load of Berkovich indenter force from 2 to 50 mN.
-
Mechanical properties of single V2O5 nanocrystal - nanoindentation measurement in control of the max-depth
Open Research DataThe DataSet contains the nanoindentation curves (indentation force Fn vs penetrationPd) for a single V2O5 nanocrystal supported on a substrate. The measurements were performed in control of the maximum depth of Berkovich indenter penetration: 60, 70, and 100 nm.
-
Results of nanoindentation, XRD and microscopic studies of bacterial cellulose
Open Research DataThe archive contains the results of research on BNC bacterial biocellulose, which was modified in two ways. When BNC was synthesized, it was subjected to in situ modification involving the addition of hyuloronic acid to the bacterial medium. The second way of ex situ modification consisted of soaking the BNC in water and then convectionally drying it...
-
Nanoindentation tests of the hydroxyapatite composite coatings applicated on titanium alloys by the electrophoretic method
Open Research DataCurrently, there are no metal materials that meet all biomechanical and biochemical requirements needed for long life implantable biomaterials. The main purpose of the study was to functionalize the surface of the titanium alloys used in biomaterial implants.
-
The influence of the temperature treatment method on the quality of French fries.
Open Research DataThe video presents instructional work on the temperature treatment of French fries and the assessment of oil changes during frying. The results of the measurements show that placing the fries in cold oil, heating them to the frying temperature compared to the conventional method of frying, reduces the amount of primary oxidation products and free fatty...
-
Laser microscope profilometry of (Ce0.80Gd0.20)O1.90 surface before polishing
Open Research DataThe dataset consists of a surface image and topography obtained using a Keyence VK-X1000 confocal laser microscope for (Ce0.80Gd0.20)O1.90 substrate (CGO-20). Imaging was performed to determine surface roughness. The Keyence VK-X1000 uses a 404 nm laser to map and measure the surface of samples via confocal scanning or a wide-field variable focus. The...
-
Partial PLA composite surface activation by femtosecond laser ablation
Open Research DataThe dataset contains the studies on electrochemical activity of PLA composite (commercially available CB-PLA Protopasta), which was 3D printed in a form of 1x1cm electrodes. The electrodes were submitted to femtosecond laser ablation operating with different parameters. These were: gas atmosphere (He or air, data in different subfolders), the percentage...
-
Data from terrestrial laser scanning: The Forge in the district of Gdańsk Orunia
Open Research DataWithin the frames of the use of terrestrial laser scanning we find numerous examples of registration of building facilities, including also historical and valuable in their culture. Data were acquired using a Leica Geosystems C10 laser scanner. Data embrace blacksmith forges a historic building located in Gdańsk Orunia, 10 Goscinna Street. Scanning...
-
Measurement of the temperature change of PVCP tissue phantom illuminated by dermatological laser 1.series
Open Research DataApplication of laboratory set-up for characterization of thermal properties of optical tissue phantoms during laser irradiation is presented. The produced system utilizes a thermographic camera VIGOcam v50 and a dermatological laser system with a 975 nm diode laser module. The set-up was used to perform measurements of the temporal and spatial temperature...
-
Measurement of the temporal and spatial temperature distribution on the surface of PVCP tissue phantom illuminated by laser.
Open Research DataApplication of laboratory set-up for characterisation of thermal properties of optical tissue phantoms during laser irradiation is presented. The produced system utilizes thermographic camera VIGOcam v50 and dermatological laser system with a 975 nm diode laser module. The set-up was used to perform measurements of the temporal and spatial temperature...
-
Generation of inhibitory compounds during pre-treatment of lignocellulosic biomass
Open Research DataDataset contains calibration curves and typical resultsa obtained during biomass pre-treatment. Data are converted from digital raw files to xlsx files
-
X-ray Photoelectron Spectroscopy studies of laser-induced titania nanotubes
Open Research DataThis dataset contains the results of high-resolution XPS studies obtained during the formation of the hollow nanopillar arrays through the laser-induced transformation of titania nanotubes.
-
The topography of carbon black-polylactide composite 3D printed electrodes after femtosecond laser ablation
Open Research DataThis dataset contains a series of scanning electron microscopy images revealing the topography of 3D printed carbon black-polylactide composite electrodes after laser ablation with a femtosecond laser. Different laser powers were investigated, namely: 10%, 25%, 50%, 75% and 100%. The CB-PLA electrodes were 3D printed using an Ender printer. Femtosecond laser NKT Photonics, Origami XP parameters: power at 100%...
-
A set of data constituting the basis for the publication entitled "Mitochondria dysfunction is one of the causes of diclofenac toxicity in the green alga Chlamydomonas reinhardtii"
Open Research DataNon-steroidal anti-inflammatory drugs (NSAIDs), such as diclofenac (DCF), form a significant group of environmental contaminants. When the toxic effects of DCF on plants are analyzed, authors often focus on photosynthesis, whilemitochondrial respiration is usually overlooked. Therefore, an in vivo investigation of plant mitochondria functioning under...
-
Laser microscope profilometry of SrTi0.3Fe0.7O3-d electrode surface after quickly drying
Open Research DataThe dataset consists of a surface image, topography and profilometry obtained using a Keyence VK-X1000 confocal laser microscope for SrTi0.3Fe0.7O3-d electrode (STF70). Imaging was performed to determine surface roughness. The Keyence VK-X1000 uses a 404 nm laser to map and measure the surface of samples via confocal scanning or a wide-field variable...
-
Laser microscope profilometry of SrTi0.3Fe0.7O3-d electrode surface after slowly drying
Open Research DataThe dataset consists of a surface image, topography and profilometry obtained using a Keyence VK-X1000 confocal laser microscope for SrTi0.3Fe0.7O3-d electrode (STF70). Imaging was performed to determine surface roughness. The Keyence VK-X1000 uses a 404 nm laser to map and measure the surface of samples via confocal scanning or a wide-field variable...
-
Laser microscope profilometry of (Ce0.80Gd0.20)O1.90 after ∼3 μm surface finish
Open Research DataThe dataset consists of a surface image and topography obtained using a Keyence VK-X1000 confocal laser microscope for (Ce0.80Gd0.20)O1.90 substrate (CGO-20). Imaging was performed to determine surface roughness. The Keyence VK-X1000 uses a 404 nm laser to map and measure the surface of samples via confocal scanning or a wide-field variable focus. The...
-
Raman spectroscopy analysis of poly(lactic acid)-carbon black composite treated by femtosecond laser
Open Research DataThe dataset contains the Raman spectroscopy measurements of commercially available carbon black-filled poly(lactic acid) 3D printed electrodes after femtosecond laser ablation. These results were utilized in the manuscript published in Electrochimica Acta: 10.1016/j.electacta.2022.140288
-
Maximum temperature of 0.5-W infrared laser-Illuminated gold nanorod platforms
Open Research DataData concern a system consisted of two pieces of borosilicate glass surrounded by air and joined together by a transparent glue, which is to serve as a thermal transducer. On the top and bottom sides of the smaller piece, gold nanorods are dislocated. Glass is prepared here due to its high transparency, facilitating heat to be produced within the system....
-
Analysis of cellular senescence following anthraquinone treatment in A549, H226, and H460 cells
Open Research DataThe datasets comprise microscopic images of A549, H226, and H460 cells following treatment with anthraquinones and staining with senescence-associated β-galactosidase. The images were captured using an Olympus BX60 microscope (Tokyo, Japan).
-
Partial PLA composite surface activation by femtosecond laser ablation
Open Research DataThe dataset contains the studies on electrochemical activity of PLA composite (commercially available CB-PLA Protopasta), which was 3D printed in a form of 1x1cm electrodes. The electrodes were submitted to femtosecond laser ablation, etching a certain % of the electrochemically-exposed electrode size. The % value is in the name of each file. The goal...
-
Raman studies of 3D printed CB-PLA samples after microwave treatment
Open Research DataThis dataset contains Raman spectroscopy analyses of microwave-activated carbon-black doped polylactic acid 3D printed electrodes.
-
Electrochemical studies of Boron-Doped Diamond enriched Laser Induced Graphene structures
Open Research DataThis dataset contains electrochemical studies aimed to evaluate the capability of the utilization of laser-induced graphene (LIG) with incorporated boron-doped diamond nanowall (BDNW) hybrid nanostructures for microsupercapacitors. Selected results from this dataset were published in Advanced Functional Materials journal: https://doi.org/10.1002/adfm.202206097
-
Scanning electrochemical micrographs of poly(lactic acid) 3D printed electrodes ablated by femtosecond laser
Open Research DataThe dataset contains the scanning electrochemical micrographs of the femtosecond laser (FSL) ablation at the surface of commercially available carbon black-filled poly(lactic acid) 3D printed electrode. The process is used for the increase of the charge transfer of this electrode in electrochemical studies.
-
Particle size distribution (laser granulometry) of pristine bismuth oxide (Bi2O3) and gadolinium oxide (Gd2O3) structures
Open Research DataData contain raw results of particle size distribution (by volume) of Bi2O3 and Gd2O3 particles determined using a laser diffraction method (Malvern Mastersizer 2000, Worcestershire, UK).
-
Optimization of the femtosecond laser impulse for excitation and the spin-orbit-mediated dissociation in the NaRb molecule
Open Research DataHigh accuracy ab initio potential energy curves (1tSigma+, 2sSigma+, 1tPi), electronic transition dipole moment function (1tSigma+ - 1tPi), and spin-orbit coupling (2sSigma+ - 1tPi) have been calculated for the NaRb molecule. The time-dependent excitation and dissociation processes in the polar alkali diatomic NaRb molecule and the quantum properties...
-
XRD patterns of the V2O5 nanorods after thermal treatment under reducing atmosphere
Open Research DataThe DataSet contains the XRD patterns of V2O5 nanorods after thermal treatment under a reducing atmosphere. Samples were annealed at 450C for 2, 20, and 40h under a reducing atmosphere (94% Ar, 6% H2).
-
Caffeine detection using CB-PLA electrode after Nd:YAG laser ablation in He atmosphere
Open Research DataThe dataset contains electrochemical studies in form of cyclic voltammetry (CV) and differential pulse voltammetry (DPV) of laser-activated 3D printed CB-PLA electrodes. The ablation of the 3D-printed CB-PLA electrodes was carried out using a pulsed LaserBlast 500 Nd:YAG laser (Quantel, France) operating at 1064 nm and a 6 ns pulse duration.
-
Images revealing the effect of local femtosecond laser ablation of conductive poly(lactic acid) 3D printed electrodes
Open Research DataThe dataset reveals the images of the femtosecond laser (FSL) ablation at the surface of commercially available carbon black-filled poly(lactic acid) 3D printed electrode. The process is used for the increase of the charge transfer of this electrode in electrochemical studies.
-
SEM micrographs of the V2O5 nanorods after thermal treatment under reducing atmosphere
Open Research DataThe DataSet contains the SEM micrographs of V2O5 nanorods after thermal treatment under a reducing atmosphere. Samples were annealed at 450C for 2, 20, and 40h under a reducing atmosphere (94% Ar, 6% H2).
-
SEM micrographs of 3D printed CB-PLA samples topography after microwave treatment
Open Research DataThis dataset contains the SEM micrographs of carbon-black doped polylactic acid 3D printed electrodes, after microwave treatment to activate the electrode surfaces. FEI Quanta 250 FEG SEM was used for these analyses. Samples were treated with CEM reactor or microwave oven.
-
XRD and electrochemical results for MoO3 films deposited using pulsed laser deposition system
Open Research DataThe attached data contains XRD and electrochemical results for MoO3 films deposited on fluorine-doped tin oxide glasses. Films were deposited using a pulsed laser deposition system at different conditions. Part of the samples was deposited at room temperature and then annealed at 575°C for given times (samples labeled PLD_RT_575C_xmin, where x stands...
-
XRD patterns of the V2O5 coatings after thermal treatment under reducing atmosphere
Open Research DataThe DataSet contains the XRD patterns of V2O5 coatings on the silicon substrate after thermal treatment under a reducing atmosphere. Thin films were annealed at 500C, 600C, and 700C for 10 under a reducing atmosphere (94% Ar, 6% H2).
-
SEM micrographs of the V2O5 coatings after thermal treatment under reducing atmosphere
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 coatings on the silicon substrate after thermal treatment under a reducing atmosphere. Thin films were annealed at 600C and 700C for 10 under a reducing atmosphere (94% Ar, 6% H2).
-
Measurements of guided wave propagation in CFRP/steel adhesive joints obtained by scanning laser vibrometry
Open Research DataThe DataSet contains guided wave signals measured in adhesive joints of steel plates (steel of type S355 with a thickness of 11.9 mm ) and carbon fibre reinforced polymer (CarboDur S1012 with a thickness of 1.24 mm). The samples were as follows: #0 – intact; #1 – 10% disbond; #2 – 20% disbond; #3 – 50% disbond; #4 – 80% disbond; #5 – 100% disbond.
-
Laser scanning point clouds of a 32-meter radiotelescope located in the radioastronomical observatory in Piwnice (Poland)
Open Research DataThis dataset contains laser scanning point clouds of a 32-meter RT4 radiotelescope located in the radioastronomical observatory in Piwnice in Poland. Measurements were performed on 18th May 2018 using two laser scanners: Leica P40 (shared by Leica Geosystems Poland) and Riegl VZ400 (shared by Geotronics Dystrybucja Sp. z o.o.). The cloud points from...
-
Terrestrial Laser Scan and Survey Images - 3D Model - Submarine Kobben - Canon - Reigl
Open Research DataDataset description: Raw images from photogrammetric and terresttial laser scaning survey. Object: Submarine Kobben - decomisionedLocation: Gdynia, Pomorskie, PolandDrone type: n/a (Teresstrial images)Flight plan: Free - walk arround the objectTarget Product: 3D ModelDate: 05.07.2017Direct georeferencing: noMetadata data: NoGCP: N0 - some targets on...
-
Terrestrial Laser Scan and Survey Images - 3D Model - Palm House - MP1 - Leica
Open Research DataDataset description: Raw images from photogrammetric and terresttial laser scaning survey. Object: Palm House in Gdansk Oliwa ParkLocation: Gdansk, Pomorskie, PolandDrone type: DJI Mavic Pro 1Flight plan: Circle | Point Of InterestTarget Product: 3D ModelDate: 06.11.2018Direct georeferencing: yesMetadata data: Yes/GPSGCP: NoCamera Name: DJI FC220Lasser...
-
Terrestrial Laser Scan and Survey Images - 3D Model - Simulated Car Accident - MP1 - Reigl
Open Research DataDataset description: Raw images from photogrammetric and terresttial laser scaning survey. Object: Simulated Car AccidentLocation: Puck Pomorskie, PolandDrone type: DJI Mavic Pro 1Flight plan: Circle | Point Of InterestTarget Product: 3D ModelDate: 07.07.2017Direct georeferencing: yesMetadata data: Yes/GPSGCP: Yes - some targets on the object are marked...
-
Floating treatment wetland with Equisetum hyemale - performance in nutrients and potentially toxic elements removal
Open Research DataThis data set contains the results of a microcosm experiment with floating treatment wetlands (FTW) conducted under artificial conditions. The goal of this experiment was to determine the effect of stress factors (Pb, As, increased salinity) on the nutrient uptake capacity of Equisetum hyemale in FTW. The ability of E.hyemale to uptake Pb and As was...
-
AFM images of the platinum (111) single crystal surface as delivered, without the polishing treatment
Open Research DataPlatinum (111) single crystal surface images as delivered, without polishing treatment. Topographic measurements in contact mode. NTEGRA Prima (NT-MDT) device. CSG probe 10.
-
Flow cytometry analysis of DNA DSBs in telomerase positive and negative cell lines after treatment with TXT2 and TXT4
Open Research DataFlow cytometry analysis of DNA DSBs in telomerase positive (A549, H460) and negative (NHBE2594, U2OS) cell lines after treatment with equitoxic concentrations of TXT2 and TXT4. MTX and DMSO were used as positive and negative controls, respectively.
-
RSM for pre-treatment optimisation
Open Research DataBox Behnken Design was prepared to define optimal contitions for biomass pretreatment
-
Light microscopy observation of emergent macrophytes in floating treatment wetlands combined with microbial fuel cells (FTW-MFC): heavy metals loaded treatments
Open Research DataThis dataset presents the light microscope images of emergent plants (Phragmites australis and Iris pseudacorus) used in floating treatment wetlands combined with microbial fuel cells (FTW-MFC) systems for wastewater treatment and bioenergy generation.
-
The BDD electrodes wettability modification by anodic polarization treatment
Open Research DataThe dataset contains the raw images, photographs obtained for the contact angle measurement at the surface of the boron-doped diamond (BDD) electrode. The measurements were carried out on after potentiodynamic polarization procedure, at various anodic polarization scan range (no polarization - HTBDD; 1.0 V; 1.4 V; 1.9 V; 2.5 V vs Ag|AgCl, scan rate...